Skip to content
PVSensors

Direct conversion

Semiconductors make charge.

In a direct-conversion detector the photon's energy creates electron-hole pairs right where it is absorbed. A bias voltage sweeps electrons to the anode pixels and holes to the cathode; the moving charge is the signal. One step - no light, no spreading.

photon → E / W electron-hole pairs → drift in the electric field → pixel electrode → ASIC

loading interactive lab…

Physics

What makes a good direct converter?

The ideal material is dense and high-Z (stopping power), has a wide enough band gap for low leakage at room temperature, and lets carriers travel far before they are trapped (high μτ).

High Z, high density

Pb, Bi, Cd, Te, Cs, I absorb X- and gamma-rays in mm, not cm.

Band gap 1.5-2.5 eV

Small enough for many pairs, large enough for low thermal leakage without cooling.

High μτ

Mobility × lifetime ≥ 10⁻³ cm²/V lets charges cross mm-thick crystals.

High resistivity

≥ 10⁹-10¹⁰ Ω·cm keeps dark current and noise low under hundreds of volts.

N = E / W → 662 keV in CZT: 662 000 / 4.6 ≈ 144 000 pairs, FWHMstat = 2.355·√(F/N) ≈ 0.2 %
W: mean energy per electron-hole pair, F: Fano factor (≈0.1). Compare with ~2 000-20 000 photo-electrons per MeV in scintillators.

Lab 1

Absorption of direct converters.

Bare silicon is the low-Z reference. Notice the Cd/Te K-edges (~27-32 keV) and the Pb K-edge at 88 keV in the perovskites.
loading interactive lab…

Lab 2

Band gap, pair energy and leakage.

Klein's rule links the pair-creation energy to the band gap. Move the temperature to see why germanium must be cooled and wide-gap materials need not.
loading interactive lab…

Lab 3

Getting the charge out.

The Hecht equation: carriers that are trapped before reaching the electrode lose part of the signal. In CZT holes are slow - small pixels fix this. Balanced μτ in perovskites helps planar devices.
loading interactive lab…

Lab 4

Thickness and resolution.

Thickness for 90 % absorption and the statistical limit of energy resolution from E/W pairs.
loading interactive lab…
loading interactive lab…

Perovskites

Lead-bromide perovskites: the newcomers.

ABX₃ crystals with A = Cs⁺ or formamidinium (FA⁺), B = Pb²⁺ and X = Br⁻. Wide band gap (~2.2-2.3 eV), high Z and balanced electron/hole transport - grown from the melt (CsPbBr₃) or from solution below 100 °C (FAPbBr₃).

CsPbBr₃

All-inorganic, melt-grown

  • Bridgman ingots up to 1.5″ diameter; zone refining removes impurities
  • 0.79 % FWHM at 662 keV (guard ring), 0.86 % at 1332 keV (ring-drift)
  • Hole μτ up to ~10⁻² cm²/V, lifetime up to ~300 µs; W ≈ 5.3 eV
  • 2.2 cm thick virtual-Frisch-grid detectors: 1.5-2.2 % at 662 keV
  • Planar devices match CZT below 0.5 MeV and beat it above 1 MeV

FAPbBr₃

Hybrid, solution-grown

  • Grown from solution below 100 °C - cheap, cm-size crystals
  • Surface passivation: 5.7 % → 1.7 % at 662 keV, near-unity charge collection
  • Br₂ during growth cuts Br vacancies ~1000× → 0.7 % at 662 keV
  • FA/Cs alloy: balanced μτ (2.2-3.2)×10⁻³ cm²/V, ρ ≈ 10¹⁰ Ω·cm
  • Photon-counting X-ray: iodine K-edge contrast at low dose

Device engineering

What made the progress

  • Asymmetric / Schottky contacts (Ga, Bi | Au, Pt) for low dark current
  • Unipolar hole-only readout: pixels, ring-drift, virtual Frisch grid
  • Blocking & passivation layers (TiC, Al₂O₃) against polarisation
  • Encapsulation (wax, ALD Al₂O₃) for months of stable bias
  • X-ray photon counting at ~0.4 Mcps/pixel; Br₂-doped crystals as 350 ps scintillators
YearMaterial / deviceResultSource
2018CsPbBr₃, Bridgman, Ga/Au planar3.8 % at 662 keV, 3.9 % at 122 keV; μτ(h) 1.3×10⁻³ cm²/VHe et al., Nat. Commun. 9, 1609
2021CsPbBr₃, 1.5″ ingots, hole-only1.4 % at 662 keV; μτ(h) 8×10⁻³ cm²/V; stable 18 monthsHe et al., Nat. Photon. 15, 36
2023FA₀.₉Cs₀.₁PbBr₃, solution-grown2.9 % at 662 keV; >65 % of crystals spectroscopicZhao et al., Nat. Photon. 17, 315
2024FAPbBr₃, NH₄Br-passivated surface1.7 % at 662 keV; dark counts ↓60×; works >130 °CZhao et al., Nat. Photon. 18, 250
2024CsPbBr₃, EFG-grown, X-rayρ 1.6×10¹⁰ Ω·cm; 46 180 µC Gy⁻¹cm⁻²; LoD 10.8 nGy/sHua et al., Nat. Photon. 18, 870
2025CsPbBr₃, virtual Frisch grid, 2.2 cm1.5 % (10 mm) and 2.2 % (22 mm) at 662 keV, digital pulse processingQin et al., Nat. Commun. 16, 158
2025FAPbBr₃, Br₂ defect healing0.7 % at 662 keV; X-ray photon countingLi et al., Nat. Mater. 24, 1993
2025CsPbBr₃ planar vs CZTBetter than CZT above 1 MeV; 225 days stableBayikadi et al., Adv. Mater. 37, e10931
2026CsPbBr₃, zone-refined Bridgman0.79 % at 662 keV; 0.86 % at 1332 keVGrundmanis et al., NIM A 1084; Crystals 16, 712
2026CsPbBr₃ X-ray photon counting~420 kcps/pixel; 2.9 % at 122 keV; K-edge imagingBayikadi et al., ACS Energy Lett. 11, 5801

Room-temperature, best reported values from each paper.

Open questions

Ion migration under bias (polarisation at the anode), slow "bias conditioning" of the spectrum, bromine-vacancy recovery during storage and contact chemistry still decide whether perovskites can replace CZT in products. What to measure on every crystal: μτ for electrons and holes, resistivity, dark-current drift, energy resolution vs time under bias, MTF and DQE.

Data

Semiconductor properties.

MaterialFormulaρ g/cm³Z effBand gapW (eV/pair)Pairs per MeVNotes
Silicon (photodiode)Si2.33141.12 eV3.62276,243Excellent for light and soft X-rays; Z = 14 is too light to stop hard X/γ-rays.
a-SeSe4.28342.2 eV4522,222Direct-conversion mammography panels. W ≈ 45 eV at typical fields.
HPGeGe5.32320.67 eV2.96337,838Best energy resolution, but must be cooled to ~77 K.
CdTeCdTe5.8550.21.44 eV4.43225,734Photon-counting CT and X-ray spectroscopy; room temperature.
CdZnTe (CZT)Cd0.9Zn0.1Te5.7849.91.57 eV4.6217,391Room-temperature gamma spectroscopy, cardiac SPECT, PCD-CT.
CsPbBr₃CsPbBr34.5562.22.25 eV5.3188,679All-inorganic halide perovskite: high Z (Pb, Cs), melt-grown (Bridgman, zone-refined) crystals; 0.8-1.4 % FWHM at 662 keV, hole μτ up to ~10⁻² cm²/V, W ≈ 5.3 eV measured.
FAPbBr₃ *CH5N2PbBr33.861.42.25 eV6.9144,928Formamidinium lead bromide: solution-grown below 100 °C; 0.7 % FWHM at 662 keV after Br₂ defect healing, balanced μτ ≈ 2-3×10⁻³ cm²/V; also photon-counting X-ray (iodine K-edge).

Z eff: power-law effective atomic number for photo-absorption, computed from the composition. * FAPbBr₃ W-value is an estimate (Klein rule); CsPbBr₃ W ≈ 5.3 eV is measured.

Compare with indirect conversion