Scintillators make light.

A scintillator absorbs the X-ray or gamma photon and re-emits its energy as a short flash of visible light. A photodetector - photomultiplier, SiPM or silicon photodiode - turns that light into an electrical pulse. Two steps, each with its own losses.

photon → electrons & holes in the crystal → activator (Tl⁺, Ce³⁺) → light → photodetector

loading interactive lab…

Physics

From a photon to a flash.

The energy deposited by the photo- or Compton electron excites thousands of electron-hole pairs in the crystal. They migrate to activator ions (Tl⁺ in NaI and CsI, Ce³⁺ in LaBr₃ and LYSO) which relax by emitting light.

Stopping power

Density and Z decide how thick the crystal must be (BGO, LYSO, GOS are the densest).

Light yield

Photons per MeV: more light → more photo-electrons → better energy resolution.

Decay time

How fast the light comes out: sets count rate, pile-up and PET timing.

Emission spectrum

Must match the photodetector: blue for PMTs, green for silicon photodiodes.

Npe = E · Y · ηcoll · QE → e.g. 662 keV in NaI(Tl) with a PMT: 0.662 × 38 000 × 0.8 × 0.27 ≈ 5 400 photo-electrons
Y: light yield (photons/MeV), η: light collection, QE: photodetector efficiency. The statistical limit of resolution is ≈ 2.355/√Npe.

Lab 1

Absorption of the scintillators.

Bare silicon is included as the reference. Switch on “only photo-absorption” to see how often the full energy is absorbed in one step.
loading interactive lab…

Lab 2

Bright or fast?

LaBr₃ is both bright and fast; BGO is dense but dim; CsI is very bright but slow; GOS is used where speed does not matter (X-ray screens).
loading interactive lab…

Lab 3

Match the light to the photodetector.

The same crystal gives a different signal with a different photodetector: CsI(Tl) glows green, where silicon is best and bialkali PMTs are weak.
loading interactive lab…

Photomultiplier (PMT)

Photocathode + dynode chain, gain ~10⁶, very low noise, ns timing. Bulky, ~1 kV, magnetic-field sensitive. Standard for NaI spectrometers.

SiPM

Array of Geiger-mode avalanche micro-cells, gain ~10⁶ at 30-60 V. Compact and MRI-compatible - used in modern TOF-PET. Dark counts and crosstalk.

Silicon photodiode

No gain but QE up to 80-90 % in the green. Cheap and stable - used under CsI(Tl) in X-ray panels and handheld spectrometers.

Lab 4

Silicon alone vs scintillator + silicon.

A scintillator in front of the photodiode absorbs what silicon would let through; the price is the light → charge step.
loading interactive lab…

Lab 5

Thickness and resolution.

How thick each scintillator must be to stop 90 % - and the best energy resolution its photo-electron statistics allow.
loading interactive lab…
loading interactive lab…

Data

Scintillator properties.

ScintillatorFormulaρ g/cm³Z effLight yield /MeVDecayEmissionNotes
NaI(Tl)NaI3.6749.738,000230 ns415 nmClassic gamma spectroscopy, SPECT cameras; hygroscopic.
CsI(Tl)CsI4.515454,0001 µs550 nmBright, green light ideal for Si photodiodes; X-ray flat panels.
LaBr₃(Ce)LaBr35.0845.263,00016 ns380 nmBest-resolution scintillator (~3 % at 662 keV); fast.
BGOBi4Ge3O127.1371.58,200300 ns480 nmVery dense, high Z, but dim. PET, Compton suppression.
LYSO(Ce)Lu1.8Y0.2SiO57.162.330,00040 ns420 nmDense and fast: the standard for time-of-flight PET.
GOS (Gd₂O₂S:Tb)Gd2O2S7.3459.460,000600 µs545 nmCeramic/powder screens for X-ray and CT detectors.
Plastic (PVT)C9H101.035.710,0002.4 ns425 nmCheap, large, fast - but low Z: almost no photopeak.

Compare with direct conversion

See the same quantities for silicon, CZT, HPGe and perovskites on the semiconductors page, or everything together on the comparison page.